Honduras T56*32*18 Manganese-Zinc Ferrite Magnetic Ring
Category:
Product Description
Communication Material Data Sheet
| Material | BMR5K | BMR5KZ | BMR7K | BMR10K | BMR12K | BMR15K | ||
| Temp. | Unit | |||||||
| Initial Permeability | 25℃ | 5000 ±25% | 5500 ±25% | 7000 ±25% | 10000 ±30% | 12000 ±30% | 15000 ±30% | |
| tanδ/μi Relative Loss Factor | 25℃ | 10 -6 | <2.0 | <6.0 | <3.5 | <5.0 | <2.0 | <8.0 |
Saturation Magnetic Flux Density (1200A/m) | 25℃ | milliTesla | 420 | 410 | 380 | 380 | 360 | 350 |
| 100℃ | / | / | / | / | / | / | ||
| Residual Magnetic Flux Density | 25℃ | 70 | 80 | 70 | 80 | 100 | 110 | |
| 100℃ | / | / | / | / | / | / | ||
| Coercive Force | 25℃ | A/m | 6 | 6 | 6 | 5 | 5 | 5 |
| 100℃ | / | / | / | / | / | / | ||
| Hysteresis Material Constant | 25℃ | 10 -6 milliTesla | <0.2 | <0.6 | - | - | <0.3 | <0.3 |
| Curie Temperature | ℃ | 155 | 150 | 130 | 125 | 120 | 115 | |
| Resistivity | Ω·m | 0.6 | 0.8 | 0.6 | 0.4 | 0.3 | 0.2 | |
Density | kg/m3 | 4.9 | 4.9 | 4.9 | 4.9 | 4.9 | 4.95 | |
| Model Name | A | B | C |
|---|---|---|---|
| T56*32*18 | 56.0±1.2 | 18.0±1.2 | 32.0±1.2 |